PAS-17 Large MLCC across a battery or unfused high-energy input with standard termination

Severity Status Implementation
warning planned mid, depends on NET-5, NET-23, NET-24, CFG-7

Looks at. The capacitor's case and termination, whether the net is battery-direct or unfused.

What it catches. MLCCs of 1206 and larger (1210, 1812, 2220 especially) connected directly across a battery or a high-energy input with no fuse between, built with standard terminations.

Why it matters. Board flexure (depaneling, screws, connectors, a dropped device) cracks large ceramics (TDK: a standard 3216 part cracks at about 4 mm of board flex, a soft-termination part takes twice that); a crack through the electrodes is a resistive short. On a source that can deliver tens of amps the cracked capacitor heats until it burns the board. Flexible (soft) terminations absorb the bend, fail-open designs and series-stacked capacitors turn the crack into an open or a half capacitor.

Example. A 22 µF 1210 X7R directly across a 2S lithium pack: a crack after a drop test smoulders.

How to check. For capacitors with role BatteryDirect or on an input with no fuse or current limit between it and the source, report case 1206 and up without a soft, flex or fail-open termination (series table, termination). Distance to the board edge, V-scores, screws and connectors is a layout check (LAY).

Fix. A soft or flexible termination (KEMET FT-CAP, TDK soft termination) or open-mode part, two capacitors in series, a fuse, smaller cases, and placement away from flex points.

References. TDK-FLEX; KEM-FLEX.