PAS-39 Iron-powder inductor run hot: thermal ageing¶
| Severity | Status | Implementation |
|---|---|---|
| warning | planned | hard, depends on NET-24, CFG-2, RPT-3 |
Looks at. The inductor's core material, its operating temperature (ambient plus losses) and the product life.
What it catches. Inductors with iron-powder cores bound by an organic binder (and moulded composite parts of that construction) whose core runs hot (ambient plus core and copper losses) for long, especially with high core loss.
Why it matters. The organic binder ages at temperature: eddy-current loss rises, permanently, after hundreds or thousands of hours, and the rising loss heats the core further, up to thermal runaway. Micrometals asks for it to be considered at or above 75 °C; Coilcraft reports competitors' iron-powder parts with five times the core loss after 1500 h at 155 °C; Würth notes the effect passes AEC-Q200 tests unnoticed because inductance stays within ±20 % while Q drops. Ferrite and some composite materials do not age this way.
Example. An iron-powder inductor in a 105 °C ambient converter with core loss comparable to copper loss: after two years in the field its losses have tripled.
How to check. For power inductors whose series or core material is iron powder with organic binder, estimate the core temperature (RPT-3 losses, the board's ambient and life_years intents; not run without them) and report above a threshold (default 100 °C) over the product's life; a series datasheet that states no thermal ageing clears it.
Fix. A core material without thermal ageing, a larger part with lower loss, or a lower core temperature.
References. MMcat; CC1192; WE128.